Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃

Brand Name : Torich

Model Number : Inconel X-750

Certification : CE PED

Place of Origin : China

MOQ : 1000kg

Price : 6000-20000 USD per ton

Payment Terms : L/C, T/T

Supply Ability : 200 tons per year

Delivery Time : 6-8 weeks

Packaging Details : In bundles in wooden box

Material : InconelX-750

Standard : AMS 5542,AMS 5598

Application : Industry

Grade : alloy

Type : Nickel Pipe

Contact Now

Inconel Steel Tue are produced with Inconel Alloy Steel Grade InconelX-750

Mechanical component

C:≤0.08

Cr:14.0-17.0

Ni+Co:≥70.0

Al:0.40-1.00

Ti:2.25-2.75

Fe:5.00-9.00

Nb+Ta:0.70-1.20

Co:1.00max

Mn:1.00max

Si:0.50max

S:0.010max

Cu:0.50max

P:0.015max

Data for material physical properties:

Desity : 0.299lbs/in3,8.28g/cm3

InconelX-750 thermal conductivity

θ/℃ 50 100 300 500 900

λ/(W/(m·℃))

14.7 15.9 20.1 25.1 37.3

InconelX-750 line expansion coefficient

θ/℃ 20~200 20~300 20~400 20~500 20~600 20~700 20~800
α/10-6℃-1 13.1 13.5 14.1 14.4 15.0 15.6 16.2

Characteristic:

InconelX-750 alloy Nickel-base superalloy.

Below 980℃ with good resistance ro corrosion and oxidation resistance

Below 800℃ has higher strength

Below 540℃ has good resistance to relaxation properties, good formability and weldability as well.

Application is aircraft engines.

Heat treatment process:

Annealing 955-1010℃,water-cooled

Weldment before welding annealing 980℃,1h

weldement stress relief annealing900℃ moisture 2h

Stress relief annealing 885℃,±15℃,24h,air cooling.

InconelX-750 mechanical properties.

σb/MPa≤965

σP0.2/MPa≤550

δ4D/%≥35

with the condition of 980 ℃ ± 15 ℃, holding the appropriate time, air cooling or rapid cooling, descaling.

σb/MPa≥1170

σP0.2/MPa≥790

δ4D/%≥15

with the condition of+ 730 ℃ ± 10 ℃, 8h, furnace cooling 55 ℃ / h or air cooling to 620 ℃ ± 10 ℃, 8h, air-cooled, the total aging time is not less than 18h

Related standard:AMS 5542,AMS 5598

Application for engine part.

Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃


Product Tags:

inconel 600 tube

      

inconel 601 tube

      
 Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃ Manufactures

Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃ Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: TORICH INTERNATIONAL LIMITED
*Subject:
*Message:
Characters Remaining: (0/3000)